bantam175uk
Electrical
We are contemplating using mating connectors plated with Cadmium (aluminium shells) in one connector and Zinc Cobalt plating on the other connector.This is a naval application in salt spray atmosphere. I don't have enough experience to be sure about the corrosive effects of these dissimilar metals. Can any one advise?
Regards.
Bantam175uk
Regards.
Bantam175uk