Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Elastoplastic Data Set From Stress-Strain Curve

Status
Not open for further replies.

wnmascare

Petroleum
Joined
May 18, 2012
Messages
37
Location
BR
Hi everyone.

I got the real stress-strain curve illustrated in the attached figure for AISI 1045 steel and I need to get the data set for an elastoplastic analysis in Abaqus, i.e., I need to get the data pairs true stress-true plastic strain.

You can observe that the curve deviates from ideal behavior, i.e., it has a plateau region at a stress level of about 500 MPa. In this case, according to standard ASTM E8E8M, two yield strengths will be obtained: upper and lower yield strengths. The red line is the line for the offset strain of 0.2%.

When we have an ideal stress-strain curve, we obtain the yield point by getting the intersection point between the 0.2% offset line and the stress-strain curve. This point will be the first one of the elastoplastic data set and the other ones can be easily calculated. Thus, my question is: how can I get the elastoplastic data set (true stress x true plastic strain) when I have a stress-strain curve which deviates from the ideal curve? Should I disregard the plateau region and translate the nonlinear portion to the point where it intersect with the linear region and then calculate the other points?

What do you guys think? Have you ever faced such situation before?

Thanks in advance. Any help will be appreciated.
 
 http://files.engineering.com/getfile.aspx?folder=0f018b2d-f0ea-4f50-8ccc-e25cf2bb9f47&file=Untitled.jpg
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top