Gents,
AH36 and EH36 are typical high tensile marine plates grades.
1) AH36 or EH 36 is not listed in ASME section IX. In case a material is not listed in ASME and you want to develop a WPS based on ASME how would you do that? What would you put as P. No. and Group No.?
2) If you have an approved WPS for ASTM A106 Grade B (I think it’s P. No. 1, Group 1) and the repair involves a high tensile marine plate (here AH 36), Is it correct to accept a mild steel WPS (as in A106 Gr. B) and based on that do a repair involving AH36 material?
Thanks and Regards
River
AH36 and EH36 are typical high tensile marine plates grades.
1) AH36 or EH 36 is not listed in ASME section IX. In case a material is not listed in ASME and you want to develop a WPS based on ASME how would you do that? What would you put as P. No. and Group No.?
2) If you have an approved WPS for ASTM A106 Grade B (I think it’s P. No. 1, Group 1) and the repair involves a high tensile marine plate (here AH 36), Is it correct to accept a mild steel WPS (as in A106 Gr. B) and based on that do a repair involving AH36 material?