EFW vs SAWL

Status
Not open for further replies.

afarboudi

Mechanical
Sep 22, 2015
14
could you please help to find out what the advantages and disadvantage of using SAWL pipes instead of EFW in a petrochemical plant is? material :A672 Gr.B60
 
Replies continue below

Recommended for you

SAW (submerged arc welding) is a type of EFW (electric fusion welding).
 