I am using Table B4.1 to determine my effective width. I have a 12guage steel plate, 120”x120”. The plate is stiffened with 3”x 1/4” bars at 24”on center. The final section will resemble the example detail in the table for cases 7 and 8. However, my question is: do I double the b value when I calculate my final section properties? I am confused because in Section B4, paragraph 2, note c, for diaphragm plates, it states that the width (b) is the distance between the adjacent lines of fasteners or welds. This gives me a large section modulus and thus a large capacity. And the (b/t) ratio exceeds the limits noted in the table. Any clarification would be greatly appreciated. Thanks.