I am looking for mechanical properties of Eccobond 285 by Henkel (formerly Emerson & Cuming). The Technical Data sheet only has density and lap shear strength. I need to have Modulus of Elasticity at least. Ultimately, I would like to investigate stress relaxation if those properties are also available.

 
Replies continue below

Recommended for you

Several years ago I was told by E&C that the eccobond 285 was "almost identical" to stycast 2850 and I have used E = 1E8 Pa. The 285 has good thermal properties since TCE is 29E-6/C. We do not use it for strenght at hi temp of 95C but it is stable. Us the 23 or 24/lv catalyst for wide temperature range.
 
Thanks jedward. At least this fills in one of the "tbd" items from the vendor data sheet.
 