Jul 15, 2005 #1 mosko Mechanical Joined Jul 15, 2005 Messages 3 Location IL What E-Modul should I use for a fiber board ?
Jul 15, 2005 #2 GBor Mechanical Joined Feb 1, 2005 Messages 1,497 Location US Could you be a little more specific? Fiber board not meaning fiber re-inforced composite material, but rather, commercial grade fiber board for construction? Upvote 0 Downvote
Could you be a little more specific? Fiber board not meaning fiber re-inforced composite material, but rather, commercial grade fiber board for construction?
Jul 16, 2005 Thread starter #3 mosko Mechanical Joined Jul 15, 2005 Messages 3 Location IL The kind that is used to make cheap furniture Upvote 0 Downvote
Jul 16, 2005 #4 GBor Mechanical Joined Feb 1, 2005 Messages 1,497 Location US Like Partical Board? Or the press board frequently used in the bottom of dresser drawers? Upvote 0 Downvote
Jul 16, 2005 Thread starter #5 mosko Mechanical Joined Jul 15, 2005 Messages 3 Location IL I guess it's press board, it's made of wood shavings pressed with some kind of glue material, but it's not an MDF board. Upvote 0 Downvote
I guess it's press board, it's made of wood shavings pressed with some kind of glue material, but it's not an MDF board.