Hi Expert,
I have some issue regarding weld overlay using ER2209 (Duplex)
Is it possible to weld overlay ER2209 direct to carbon steel (1st Layer and 2nd layer with ER2209) instead of using buffer layer ER309L (1st Layer ER309L + 2nd Layer ER2209) , Is there any Corrosion problem as per G48 Testing or A923 testing ?
I just think ER2209 have %Cr and %Ni lesser than ER309L, so may be we need buffer layer to accomodate dilution on first layer.
Thank You