We have a Sect VIII, Div 2. vessel that requires S31803 duplex material for the fittings (elbows, reducers). Our supplier wants to provide SA-815 for Div. 2 service. We have scoured the Code, Interpretations, and Code Cases for any hint that SA-815 material is permitted in Div. 2 construction but found none; it is only acceptable for Div. 1.
1. Is there a reason that SA-815 (S31803) material is not allowed for Div. 2 service? And more importantly,
2. Is there any S31803 material for fittings that can be used in Div. 2 service? We have also searched for this but found nothing.
Need some insight.