Mechanical
Feb 3, 2012
78
Can I use A182 F51 & A928 UNS S31803 material to build piping per B31.3 as same material is not reflecting in Table A
 
Replies continue below

Recommended for you

Yes.

- Steve Perry
This post is designed to provide accurate and authoritative information in regard to the subject matter covered. It is offered with the understanding that the author is not engaged in rendering engineering or other professional service. If you need help, get help, and PAY FOR IT.
 
Thanks Steve, After careful review I noticed that unlisted material can be used if these are from published specifications

cheers !!
 