Sep 24, 2007 #1 maya04 Materials Joined Nov 1, 2006 Messages 15 Location IL hi, can someone please advise the difference between matt and bright tin plating from: 1. corrosion point of view 2. soldering (still using little Pb) it is applied on aluminum for soldering thanks