Mar 2, 2011 #1 delagina Structural Joined Sep 18, 2010 Messages 1,008 Location US anyone knows where i can look to check ductility of metal deck composite to concrete slab and/or metal deck slab composite to supporting I beam? or should i be checking this at all? thanks,
anyone knows where i can look to check ductility of metal deck composite to concrete slab and/or metal deck slab composite to supporting I beam? or should i be checking this at all? thanks,
Mar 2, 2011 #2 kieran1 Structural Joined Feb 27, 2002 Messages 178 Location GB Not sure where your based, but in the UK the following covers most things Kieran http://files.engineering.com/getfile.aspx?folder=eaf9955d-fc81-4db2-88c3-7b89967ff13d&file=Design_Of_Composite_Slabs_&_Beams_with_metal_decking.pdf Upvote 0 Downvote