Ductile Iron Pipe size

Status
Not open for further replies.

Lan123

Civil/Environmental
Aug 27, 2010
155
Is 14" a common pipe size used in Ductile Iron pipes for water distribution. I know 18 inch not common pipe size. Any reason for this?
 
Replies continue below

Recommended for you

Both 14" and 18" are available standard sizes per AWWA C151 etc. standards; however, you are probably right in your sense that they are sometimes not as readily available as 12", 16", and 20" etc.
 