I would like to know where I can find density values for AHSS materials, namely for dual-phase steels.

Thanks.
 
Replies continue below

Recommended for you

People forget that all steels (From pure iron to tool steels) have density and modulus that only vary by a few percent.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 