Sep 23, 2013 #1 gtfire Mechanical Joined Feb 17, 2010 Messages 10 Location CA NFPA 13 2007 SEC 8.3.4.3 Makes reference to galvanized piping on dry systems when using k=4.2 spkr heads. Does galvanized piping mean just the pipe or the pipe and fittings
NFPA 13 2007 SEC 8.3.4.3 Makes reference to galvanized piping on dry systems when using k=4.2 spkr heads. Does galvanized piping mean just the pipe or the pipe and fittings
Sep 24, 2013 #2 cdafd Specifier/Regulator Joined Aug 18, 2005 Messages 2,953 Location US All internal portions Upvote 0 Downvote