Have poured approx 1200' paved ditch. All concrete/steel passed spec inspection. Large Paved area adjacent to 200'.
2 drain outlets from paved area about 30' from top of wall. Wall failed in this area (large longitudional crack @ approx. 3' up.) Wall 9' high on 1:1 (45 degree)slope. Fill material red clay. Compaction spec acheived. Significant rain event preceeded break. Remainder of wall no problem. Hydrologist suggests that either rain retained in equipment (Euclid trucks) ruts or equipment loads passing behind wall during construction are cause. Some agree, I doubt. Any ideas, suggestions,etc?
2 drain outlets from paved area about 30' from top of wall. Wall failed in this area (large longitudional crack @ approx. 3' up.) Wall 9' high on 1:1 (45 degree)slope. Fill material red clay. Compaction spec acheived. Significant rain event preceeded break. Remainder of wall no problem. Hydrologist suggests that either rain retained in equipment (Euclid trucks) ruts or equipment loads passing behind wall during construction are cause. Some agree, I doubt. Any ideas, suggestions,etc?