Joe,
I work for Team at a refinery in baytown. We have successfully kept a roof from sinking by using our Closed cell urethane system. As far as I know , we are the only company that has done a double deck cb&i design successfully. The fourth ring flooded and we were able to get the tank back to operation in 10 days.
The tank was never taken out of service.
dennis mccarty
api 2000
nace 111 # 806
Nace CIP instructor

 
Replies continue below

Recommended for you

Dennis:

It looks to me that this posting was intended to be a response to the following thread, which you apparently already answered to:

Pontoon Leaks
thread809-258281

If that's so, then you need to redflag this posting and ask the administrator to deleted it. Feel free to post again in the above thread if you want to add additional information.

No worries...

Mike McCann
MMC Engineering
Motto: KISS
Motivation: Don't ask
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor