lh
Mechanical
- Jul 24, 2002
- 1
I would like to blend Niobium powder (60 mesh) and Titanium sponge (1/8" minus) in a small 1 cu ft double cone blender. My question is, what is the minimum number of rotations I can expect for a decent blend? At what RPM?