<br>
<br>
domestic hot water tanks <br>
LF (Aerospace)<br>
<br>
<br>
I am not familiar with ceramics but can anyone explain to me (in<br>
laymans terms) the procedure and aparatus used to coat the inside of<br>
domestic hotwater tanks with a glass or glaze?<br>
<br>
Thanks <br>
LF
 
<br>
The easiest is to insert a rotary spray head into the tank and spray for a minute or two.<br>
<br>
I think most small tank coatings are applied with some variant of this method. <br>
<br>
Hope this is what you are looking for.
 