Does an ASTM standard exist for measuring the shear modulus of viscoelastic materials?
 
Go to <A HREF=" TARGET="_new"> and do general search in ASTM Store for individual standards. Found many citations for &quot;Shear Modulus&quot; and many for &quot;Rubber&quot;. Try ASTM D6048 for rubber properties tests.
 