GusMontiel
Mechanical
Hello all!
I designing a Pressure Vessel where the body is SA-516 70 but three nozzles would be A335-P92, A335-P1, and A335-P11 (the same material as the end-pipe connection considering the steam temp). There is an internal spray system that keeps the internal surface of the shell at 400 °C.
So my doubt is regarding the weld between these dissimilar materials:
Some experiences in plants with similar situations?
The thermal stress in the weld can lead to failure in it, what would be the recommendation for the weld and filler?
Thanks in advance!
I designing a Pressure Vessel where the body is SA-516 70 but three nozzles would be A335-P92, A335-P1, and A335-P11 (the same material as the end-pipe connection considering the steam temp). There is an internal spray system that keeps the internal surface of the shell at 400 °C.
So my doubt is regarding the weld between these dissimilar materials:
Some experiences in plants with similar situations?
The thermal stress in the weld can lead to failure in it, what would be the recommendation for the weld and filler?
Thanks in advance!