toval

Mechanical
Jul 10, 2000
2
What could be the best disposal or use of Nickel after the hydrogenation of edible oils?
 
Replies continue below

Recommended for you

I want to buy spent raney nickel catalyst
 
Fatty ni catalyst waste can be burn to recover ash that contains nickel.
For this process to be of any economic value the ash should contain minimum 15 to 20% nickel and not more than 50% burn loss
What is the nickel content on as is basis? In other words what is the % loss in weight if material is incinerated and what is the ni content in the ash?

Koshik Patel

 