Yes, if the port you install it in matches the plug and you use a sealing washer. The thread is British Standard Parallel Pipe.

Ted
 
I notice there are 2 type of sealing washers i.e aluminum and copper.
If my port material is aluminum, can i use aluminum washer too?

R.Efendy
 
I prefer a stainless steel washer with a bonded buna o-ring rather than a soft cu or al washer which must be crushed to seal.

Ted
 
thanks for your reply. Appreciate that.