Is there a reasonably close US equivalent to DIN C60N?
 
Replies continue below

Recommended for you

ASTM A 830 Number 1060 (UNS G10600)
SAE 1060
Main difference: C60N according DIN 17200 must be delivered in normalized condition (letter N), US standards permit a delivery in as-rolled condition.
 