Hey Need some help here.

The above DIN 5480 spline
18 T
2 MOD
30 Deg PA
MOW =45.122-45.045mm
wire or ball=4,500

Please advise if the major & minor dia are correct.

customer has TIP Dia : 39,60 mm
Root Dia : 35.60mm
effective root : 35.581mm-35.494mm
whole depth : .200mm

I get a Tip Dia of 38.6 mm
whole depth of 2.300 mm

also does the above MOW look correct.

Thanks
 
Replies continue below

Recommended for you

Your customer's data is correct.
WD is obviously 2mm +, not 0.20mm.
I get a slightly different tolerance for MOP 45.098 - 45.055.
Not much difference but it may be important.
I can post a data sheet if you like.

Ron Volmershausen
Brunkerville Engineering
Newcastle Australia
 
Gear cutter thanks for the reply.
yes please do post a data sheet.

as you can see I am not proficient with DIN splines.

Thanks Again

Mfgenggear
 
mfgenggear - On your print should be a description like:
DIN 5480 - 40 x 2 x 30 x 18 x 8f (or any other tol.)
DIN 5480 - dia. x modul x deg. x Nr. teeth x tol.
If you do this type of work I would advise you to get a complete copy of DIN 5480 in English from: Talk to them and ask for a copy in English. Juergen
 
Juergenwt

Thank you for your reply.

I normally work with ANSI splines
This is a first for me.
I have the DIN Specs Part 1 & 2

Thanks & Take Care

Mfgenggear
 
Here you go

GPEFDIN548040x2x30x18x9H8g.jpg


Ron Volmershausen
Brunkerville Engineering
Newcastle Australia
 
Thanks you gear cutter.

I see the root dia is different
my customer has 35.581-35.494 mm

my tool cutter expert said it should be approx. 34.938mm
which falls into your size.

I will have to have a hob modified to cut their root.

Thanks again