As for required strength (Target strength) is given as (Characterstics strength + 1.64 * S.d).. this 1.64 may vary as depending on different criteria.
I had also seen some specs defining Target mean strength with totally different calculations, i.e (0.9*Characterstics strength+2.33*S.D)