Hi experts,
Again coming with an other query, when should we use ASTM GrB7 and B7M, as far as I know the basic difference is B7M is of low tensile and yield strength, but I am confused if there are other differences as well? we have temperature between 350C-400C
Thanks
 
 
XL83NL Thanks for all the links, it really helped.
 