What is recommended tubing/hose material for DI water? I have to plumb flexible water chiller lines with a service loop to/from hot/cold plates.

David Baird
dbaird@gemcity.com

Sr Controls Engineer

EET degree.

Journeyman Electrician.
 
Replies continue below

Recommended for you

I design lasers using D/I water and typically I use clear polybraid tubing.

Let me know if I can help further. email if you'd like