The calculation method (hardenability) described in the ASTM A255 is applicable only to a range of chemical composition. Nickel max is 1,50. It is not applicable for 4340. Someone knows how can I calculate hardenability for this steel (4340)?
 
thread330-366454

thread330-288119

thread330-238962

 
I am trying use Prediction of Microstructure and Hardness in Low-Alloy Steel : The tool calculates the fractions of different ferrite morphology that forms from the austenite and relates the same to Vickers hardness
but which cooling rate is more adequate (quench in polymer)?
 
Is this for a weldment? Or is this to predict the hardness after quenching in oil/water/water+polymer/etc. You can use the ASTM A255 method to estimate the hardenability of 4340, which will likely be more accurate than the EWI method.
 