danielgp1990
Industrial
Hello everybody,
I´m having trouble with a steel cooling system because Heat Tranfer it´s not my area of expertise. First I must determine the water flow that it´s necessary to cool a 7 m^2 steel surface from 550°C to 200°C using 9 sprinklers. The steel is an A-36 12mm curved wall and water should be 20°C and the heat tranfer to the enviroment is neglectable.
Can you please help me find the proceeding that is necessary to determine the water flow. Any books or any other references would be much appreciated too.
I´m having trouble with a steel cooling system because Heat Tranfer it´s not my area of expertise. First I must determine the water flow that it´s necessary to cool a 7 m^2 steel surface from 550°C to 200°C using 9 sprinklers. The steel is an A-36 12mm curved wall and water should be 20°C and the heat tranfer to the enviroment is neglectable.
Can you please help me find the proceeding that is necessary to determine the water flow. Any books or any other references would be much appreciated too.