First, I am new at this forum and if this is in the wrong place I am Sorry.
I am work with building a proof of concept for a marine current powerpland. And right now I have come to the design of the turbine.
An overview of the device so far:
Size:
Inserts
I am a mechanical enigineer but the composite area is new to me. I have read a couple of books.
I am working in SW2010 and use the shell composite simulation
Forces and result
I am using data from Fiber Composite Analysis and Design:Composite Materials and Laminates Vol 1. Unidircectional 0.6 vf.
E-glas
Ex:45GPa
Ey,Ez:12GPa
G:4.4GPa
Vlt:0.25
T-300
Ex:132GPa
Ey,Ez:10GPa
G:6.5GPa
Vlt:0.25
Glass for the arms and Carbon for the wings.
Carbonfiber and stainless steel, can it be galvanically isolated with a layer of glassfiber?
How will water ingress in the structure and can it be avoided?
Can i combine glass and Carbon fiber in the same laminate?
What is best to use vowe or unidircetional?,
what stacking and angles sequence is best? How thick should i choose the different layes in the simulation?
How many layer are feasible to have?
I am also alooking for generell feed back, is It possible to make moldins this way?, is there a easier and better way to connect the blades?
I am work with building a proof of concept for a marine current powerpland. And right now I have come to the design of the turbine.
An overview of the device so far:
Size:
Inserts
I am a mechanical enigineer but the composite area is new to me. I have read a couple of books.
I am working in SW2010 and use the shell composite simulation
Forces and result
I am using data from Fiber Composite Analysis and Design:Composite Materials and Laminates Vol 1. Unidircectional 0.6 vf.
E-glas
Ex:45GPa
Ey,Ez:12GPa
G:4.4GPa
Vlt:0.25
T-300
Ex:132GPa
Ey,Ez:10GPa
G:6.5GPa
Vlt:0.25
Glass for the arms and Carbon for the wings.
Carbonfiber and stainless steel, can it be galvanically isolated with a layer of glassfiber?
How will water ingress in the structure and can it be avoided?
Can i combine glass and Carbon fiber in the same laminate?
What is best to use vowe or unidircetional?,
what stacking and angles sequence is best? How thick should i choose the different layes in the simulation?
How many layer are feasible to have?