A robust fabric maintenance programme is neccessary to mitigate corrosion under insulation (CUI) or corrosion under fireproofing of assests. This phase comes after the plant has been fired up.

For FEED phase, what are the parameters should I incorporate when designing for the prevent of CUI/CUF.
In other words
(a)what are the crucial key features should I be aware for vessels and piping for both high temperature and low temperature duties.

(b) are there specific designs should I avoid for vessels/piping and associates assets.

(c) when load-bearing insutlation is used. How do I determine which type of load-bearing insulation suitable for specific duties.

(d) is non-contact insulation system used for CUI/CUF prevention



Any input will be much appreciated especially site/field experience.




 
The simple answer is to adopt 'inherently safe design' principles and avoid insulation unless it is fully proven to be required.

If it is proven, then make sure that a qualified coating is selected to provide the corrosion control under the insulation, i.e. one that has demonstrated immersion performance at temperature. See the attached for further guidance.

For PFP, it depends what you pick. API Publication 2218 will run you through the pros and cons. If you go the intumescent route, take a look at TGD-11 here


(you will have to register to download)





Steve Jones
Materials & Corrosion Engineer

 
Thanks for your input..:)

Just one more question.

How would noise/vibration affect the integrity of the insulation?I can only assume this would loosen the hold of the insulation to the substrate.
 
It's the paint, or other coating, that has a 'hold' on the substrate. Vibration might affect the weatherproofing seals, but it might also cause fatigue of the piping. Which is worse?

Steve Jones
Materials & Corrosion Engineer

 
Fatigue of piping of course...:)

 