JBENGR
Industrial
- Dec 22, 2014
- 4
Is there a difference in 300# rolled grooves and what I know as Victaulic couplings? Has anyone done comparison test on performance in overpressure situations. No doubt, screw couplings are problematic; you have to go one schedule higher to ensure adequate wall thickness after the threads are cut and the threads are notorious as start points for significant corrosion over time.
If grooved is stronger than threaded, perhaps I should consider changing to grooved where we currently allow threaded, I won’t budge off butt welded flange for larger than 2” unless some really good data is available.
Any information is appreciated.
If grooved is stronger than threaded, perhaps I should consider changing to grooved where we currently allow threaded, I won’t budge off butt welded flange for larger than 2” unless some really good data is available.
Any information is appreciated.