A recent problem relates to valves supplied by a canadian valve company ( starts with a "V") for a US gas fired combined cycle plant.
Our valve spec stated "no materials sourced from China may be used ". We found the F91 forged small bore valves were stamped as forged in India, but the original bars were formed in China, then forged in India.
Is there a definition accepted as a "term of the trade" that specifies whn a substance becomes a "material"?
At other related components, we found high pressure high temp fittings recieved at the same site stamped as A182F22 but are in fact carbon steel.
Our valve spec stated "no materials sourced from China may be used ". We found the F91 forged small bore valves were stamped as forged in India, but the original bars were formed in China, then forged in India.
Is there a definition accepted as a "term of the trade" that specifies whn a substance becomes a "material"?
At other related components, we found high pressure high temp fittings recieved at the same site stamped as A182F22 but are in fact carbon steel.