Dear Sir As per NACE MR 0175/ ISO 1

Status
Not open for further replies.

mandmm

Mechanical
Joined
Apr 2, 2016
Messages
10
Location
KW
Dear Sir As per NACE MR 0175/ ISO 15156-2 CLAUSE 7.4
Is it required to carry hardness test for the material if plate cut by using gas cutting machine as per NACE requirement?
 
If the stated criterion of 7.4 for having to perform hardness testing is achieved, then, yes. Even if it is not achieved, the end user may still instigate such testing as deemed necessary.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 