DC Current/Rebar/Electrolysis

Status
Not open for further replies.

ghostbuster7

Electrical
Jun 25, 2007
80
DCNew site to be designed.

Measured 10 to 20 amps dc ground current at site.(Source of DC current will never go away and is generated by some other group).

What is the best way to protect the rebar in the concrete from electrolysis?

Epoxy coatings?

Galvanizing?

Sacrificial anodes?

Thanks
 