bigbro

Mechanical
May 20, 2006
9
we have had some small (1"nb & 1/2"nb)diameter nozzles (A106/ A333 Gr6)damaged in transit due to the nozzle being bent. My question, is there a limit to the amount the nozzle is bent before you need to replace it or attempt to straighten it mechanicaly by heating.
 
Replies continue below

Recommended for you

Perhaps you could use the criteia of ASME B&PV Code Sec VIII D1, par. UCS-79? [UHA-44 (stainless) has equations for tube/pipe.]
 
Is this on a new pressure vessel? Apparently, this is an alignment nonconformance issue and IF I were the Owner's Engineer, I would request detailed measurements of the current nozzle and have you perform surface nondestructive testing (NDT).

You have two options; either replace them or locally weld repair them, if the surface NDT is acceptable, and machine concentric.
 