Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cyrogenic Manhole

Status
Not open for further replies.

dungun

Mechanical
Dec 30, 2005
39
Hi Friend
I have problem with manhole low temperature suction drum in JT/TurboExpander section. The Design temperature minus 80C and design pressure 78barg. Operating pressure and temperature 62barg and minus 70C. Manholes 20"x600#. All Materials Stainless Steel 316. While shifting TExp to JT valve, the pressure in vessel will increased to 68barg and sabile back to 62barg, and make the Gasket burst, 4 times already happened. Anyone experience on this and what is the solution?
Thanks


 
Replies continue below

Recommended for you

A little more information please.

What type gasket?

What is the fastener torque?

Can you explain your design condition a little better?
 
RF - SPW Graphite Filler SS with Centering.
Bolt Torquing
Design Pressure : 78 barg
Design Temp : -80C
Oprating Pressure : 62barg
Operating Temp : -70C
Liquid HC Condensate Reflux and HC Gas on Top.
 