Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cutting Lifting Lug from Steam Surface condenser 1

Status
Not open for further replies.

deepu78

Mechanical
Nov 11, 2008
51
Cutting 4 lifting lug during installation due to interference with structural beam.
1. Does it affect the integrity of vessel?
2.How much protrusion should be kept after cutting?
3.Which method of cutting(oxy cutting allowed?) permitted? What precaution to be taken.
DV
 
Replies continue below

Recommended for you

Generally lifting lugs are welded on to doubler plates / reinforcing pads so no issue with the integrity of the vessel.
If welded directly to vessel oxy cutting is fine as long as you cut (3 - 6 mm / 1/8" to 1/4") above surface and then grind down from there.
Somebody needs to monitor as workers will always try to cut as close to the surface as they can to reduce grinding.
Cut too close and they may gouge into the vessel and then you have major issues.
 
DD is on the money here.
I have seen many of these partially removed, just enough to get clearance.
I would not try to grind flush, leave the original weld unless it is on a doubler.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Cut as far away from the shell as possible.