sloth4z
Mechanical
- Aug 12, 2003
- 132
Does anyone know of a good tool to cut kevlar with? It takes about twenty strokes with an exacto knife. We have used an EZcutter (i think thats the name), but it wears out the blades too quick and still doesn't cut well. Currently we use a ceramic blade. The only problem is its brittle and keeps chipping. Any suggestions?