Dear Sirs,

What kind of cutting disc to be used for the pipe (15E material)?
If we used cutting disc for carbon steel, does it affect 15E material?

Need your advise.

Thank you.
 
Replies continue below

Recommended for you

One can use abrasive cutting disks that are used on carbon an other low alloy steels.
 