kwb74
Mechanical
- Dec 7, 2004
- 6
I have been researching welding units both MIG and TIG. Something has struck me as odd everywhere I read that you must have AC to weld aluminum when discussing generalities but then getting into specs of weld units and I see DC mig machines that are quite good at Aluminum. What is it about MIG that lets DC work for it but to TIG you need AC?