Does anyone know where I can find current costs for specific sections of steel? Thank you very much!
 
Replies continue below

Recommended for you

I would call or talk to a local steel fabricator or erector to get an accurate number.

In my area (midwest states, USA), installed steel (raw steel, fabrication and erection) is running about $1,500 a ton, or $0.75/pound on jobs with a sufficeint amount of steel (whole buildings or large additions). This number can vary widely depending on location and the specific job requirements.
 
$1500/ton for erected steel would be the bargain of the millenium. Are you sure it's not material only?

We do a lot of steel projects all over the country. Average prices range from $3000-$4000 for erected steel.


I'm not sure you can get a breakdown of costs for specific sections. Granted there may be higher costs associated with handling and erection of heavy sections, and tube steel is typically 30-50% more than rolled wide flanges, but I've always seen the estimates by the ton.

Calling any fabricator would get you a quick answer for your specific area, however.

 
Thank you guys very much for your input! I will take note!
 