Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Current range value was specified in PQR when make tube to tubesheet qualification as per QW-288

Status
Not open for further replies.

Tony1t

Mechanical
Joined
Jun 18, 2012
Messages
22
Location
HK

Hi everyone,
A question was raised as current range value was specified in PQR when make tube to tubesheet qualification as per QW-288.

When I reviewed WPS for tube to tubesheet at shop found that a curent range value(235~300 A) was specified in WPS, alike a current range value (260~275 A) was also record in PQR which is used to supports the WPS. QW288.1 (m) said that a change of more than 10% in the current level from that qualified is need to requalified.

My question is that when make welding on product to use current value 300A that is exceeds the limit of 10%260A, is it acceptable to specified current range value in PQR &WPS like description above?