Hi,we are having curling problems in two of our buildings.One of the building is a refrigarator,the other one is a printing facility.
We have novocon steel fiber in both floors 30 pounds per cubic meter ,six inches slab,lazer screed,water cured for ten days,60 pounds hardener, ashford formula for sealer,water reducer"super plastifier",plastic vapor barrier.Thanks for taking the time .
In the printing facility we maintain a 45 % humidity level.
The curling started around six months after the finishing.