Is it possible to keep a concrete slab on grade (floor 4" thick) too wet after placing it? The slab was kept moist sprinkler or wetted with a hose for 3 1/2 to 4 weeks after placememt. The slab was inside a closed building and plastic was placed over the slap untill the color was uniform after the about 5 1/2 week it was removed. Problem is it has extensive shrinkage cracks contractor is arguing the floor was kept wet longer than it should have been during the curing. However the wire mesh was not held up during the poor (it was pulled up with a hook)and the two slabs 28x30 were not saw cut untill after the cracks started to appear. Any advise would be greatly appreciated.