Jul 8, 2004 #1 Robjack Mechanical Joined Jan 9, 2004 Messages 5 Location US I'm looking for CTE data on ASM 6471 steel. Does anyone have a good source?
Jul 9, 2004 #2 tbuelna Aerospace Joined Aug 10, 2002 Messages 4,026 Location US robjack: The best free online source for material properties is MatWeb: http://www.matweb.com/index.asp?ckck=1 I did a quick search for Nitralloy (135 Mod.)and its other designations (MIL-S-6709 and UNS K24065) but could not find anything listed. As for CTE values, I would guess that it is close to other low alloy steels CTE= 7 x 10-6 in/in/degF. Regards, Terry Upvote 0 Downvote
robjack: The best free online source for material properties is MatWeb: http://www.matweb.com/index.asp?ckck=1 I did a quick search for Nitralloy (135 Mod.)and its other designations (MIL-S-6709 and UNS K24065) but could not find anything listed. As for CTE values, I would guess that it is close to other low alloy steels CTE= 7 x 10-6 in/in/degF. Regards, Terry