We have a crude oil export pipeline that we want to introduce NGLs into. Is it a possibility that if we have an impact/damage which results in small ductile tear that the escaping NGLs could cause a subsequent drop in metal temperatures and potentially a brittle failure? The pipeline was designed for ambient use and there is now low temperature impact data. Is this a real concern and if so what % NGLs would be considered a problem? Any ideas/help would be appreciated.
 
Replies continue below

Recommended for you

NGL product is normally transported in carbon steel piping. Assure that the pipeline is suitable for the operating and maximum pressure. A tear in a pipeline is a serious failure, not a normal event.
 
If the pipeline has already been ruptured by means other than a brittle or ductile fracture, the driving force for crack extension should have been lost. It wouldn't be normal to compute a minimum design temperature on the basis of a pipeline rupture but the process engineers should look at the implications for a pipeline blowdown scenario. Then, in the absence of toughness data for pipe (and welds?) you may have an integrity assessment to perform.

Steve Jones
Materials & Corrosion Engineer
 