Below is a material analysis results and hope someone can help out.

C .30%
Mn .36%
P <.010
S <.001
Si .30%
Cr 12.03%
Ni .08%
Mo .27%
Cu .02%
Al <.01
Sn <.01%

Hardness 34 HRc
 
Hello,

I have never heard of Cronidur 30, but the chemistry that you supplied above is super close to AISI 420 SS (with a trace of Ni, Cu, Al and Sn). Could you give more information on chronidur 30? What is the application for this material?

Coka
 
The application is a gear. I only heard of the other material from reading a trade artical. I don't know all the properties of Cronidur 30.
 
As a casting I have produced lot of castings for paper mill applications. The only change was that Carbon was 0.35% instead of 0.3%. This can be machined and later hardened and tempered to desired hardness.
 