I have bee asked to duplicate the two crimps shown is this image:


The material is aluminum. The O.D. of the non-crimp portion is 0.224in. The I.D. of the non-crimped portion is 0.200 in.

The width of each of the crimps is about 0.25 in (1/4") and the spacing in between both crimps is about 0.250 in (1/4")

The black on the right is simply a hose placed over the un- crimped portion.

I can custom make tooling.

I could really ANY ideas on how I would do such a crimp and/or make a tool to do this. Regular crimping tools can't do this.

Any idea would be well appreciated.
 
You have to make a crimping tool in two halves as with a scissors. You will need to design the tool carefully and experiment a little to get it right making allowances for how much give is in the material. It's not my field but I have see toolmakers do it and that is something they specialise in.
 
It appears to be a rolled crimp using something like a knurling tool. The rubber is already cracked so you really do not want to use such a crimp, where the sharp edge of the ferrule cuts into the rubber.
 
Hydtools, I think you are correct. It still seems a good idea to move the crimp in a little from the end of the ferrule to reduce the sharp edge causing a stress riser in the hose wires.
 
I just need some ideas on how to put the crimps in the Aluminum. I don't care about the hose at all.

Any good suggestions would be well appreciated.
 